Ender 3 build plate temperature. by Ethan Sommer. Retraction Speed: 45 mm/s. . The print data for PLA are as follows: Extruder temperature: 190 – 220 °C. Figuring out the best PLA print and bed temperature can be tricky. As the object builds, and it gets further away from the heated build plate, the plastic gets colder and shrinks. In order to improve build plate adhesion for PLA, ABS, and PETG, you should level your build plate, optimize your build plate temperature, use an adhesive on your build plate, and adjust slicer settings such as Initial Layer Speed. Usually, you’re better off using the default temperature specified by your filament manufacturer in Cura. Print speed: 60 mm/s (recommended value) Retraction distance: 5 mm. Updated Jan 6, 2024. The print data for PLA are as follows: Extruder temperature: 190 – 220 °C. Cooling: required. The Best PLA Bed & Print Temperature Settings. It's a problem with your ambient temperature. The easiest way to fix this issue is to put your printer in an enclosure. Build Plate Temperature Initial Layer. Increase bed adhesion and/or decrease temperature gradient over the part. The build plate temperature initial layer is the temperature that the printer heats the build plate to while printing the first layer. Check out this quick guide to learn all you need to know. These factors include the surface, the temperature change during printing and the leveling of the glass bed. These basic technical characteristics are fulfilled by the Ender 3. This isolates the air immediately around the printer from the rest of the air in the room. The bottom stays warm and does not In order to determine the best options and perfect temperature setting for the Ender 3 glass bed, there are three basic factors of Ender 3* component adhesion that you have to internalize. kwlnraubcwgdusyyaexsjqlmnkmmnssrgjeumvphjedyjiveqrpz